Zanglamaydigan po'lat rulon
Sovuq prokatlangan 2B / BA va issiq prokatlangan No.1 rulon 304 / 316L / 430 / 201 — 0.3–12 mm, rulon og'irligi 20 t gacha.

304 sovuq prokatlangan zanglamaydigan po'lat rulon 2B

316L sovuq prokatlangan zanglamaydigan po'lat rulon 2B

430 sovuq prokatlangan zanglamaydigan po'lat rulon BA

201 sovuq prokatlangan zanglamaydigan po'lat rulon 2B

304 issiq prokatlangan zanglamaydigan po'lat rulon No.1

316L issiq prokatlangan zanglamaydigan po'lat rulon No.1

2205 dupleks issiq prokatlangan rulon

304 zanglamaydigan po'lat kesilgan tasma

430 zanglamaydigan po'lat aniq tasma
Mavjud spetsifikatsiya
| Markalar | Qalinligi | Kenglik / diametr | Standart |
|---|---|---|---|
| 304 · 316L · 430 · 201 | 0,3–12 mm | ≤ 1500 mm | ASTM A240 / EN 10088-2 |
Odatdagi qo'llanilishlar
- Uzluksiz shtamplash va prokatlash
- 分条与平直剪切
- 开平与定尺切割
交付与检验
- 内径 508 mm / 610 mm,卷重 3–20 t
- 纸或薄膜衬垫,可立式或卧式包装
- 可根据要求将卷内厚度差控制在 0.03 mm 以内
Typical applications
Below is where this material actually ends up — the specific parts, not just the industry. Compare it with your own service conditions, or send us the environment and we will advise.
- Kitchen equipment — sinks, hob panels, range hood shells, commercial fridge liners
- Home appliances — washing machine drums and panels, microwave cavities, steriliser racks
- Architecture — elevator door frames and car panels, façade trims, balustrades, handles
- Food and pharma — filling line tables, tank liners, cleanroom wall panels
- Consumer goods — vacuum flasks, cookware, cutlery, bathroom fittings
Selection FAQ
- Should a kitchen sink be 304 or 316 stainless?
- 304 is enough for domestic use. For coastal areas, or where salt and detergent sit on the surface, 316L lowers the pitting risk.
- What is the difference between 2B and BA finish?
- 2B is cold rolled, annealed, pickled and skin-passed — a matte silver-grey. BA is bright annealed: more reflective, closer to mirror, slightly higher cost.
- Does stainless steel rust?
- "Stainless" is relative to carbon steel. Chlorides (salt, bleach) and scratched surfaces are the main triggers; in coastal or chemical environments upgrade 304 to 316L.
Not sure which grade fits? Use the grade selector